Shanghai Bijoy Technology Co.,Ltd.
Home > Products > Welding Wires > (YongXiang) YX 50-6 CO2 Shielding Welding Wire ER50-6 (0.8Mm/1.0Mm/1.2Mm/1.6Mm)

(YongXiang) YX 50-6 CO2 Shielding Welding Wire ER50-6 (0.8Mm/1.0Mm/1.2Mm/1.6Mm)

— 50-6, welding wire, YX 50-6
Product Category: Welding Wires
Sales Method: Export, Manufacture, Wholesale
Payment Term: T/T, M/T, D/D, Check
Min. Order Unit Price
100 Pieces

Product Detail

Product Attribute:

  • China (mainland) More >
  • 50-6
  • 07/31/2013
  • 08/01/2013

Additional Info.:

  • container

Product Content Description:

Meet the criterion of GB ER50-6, and correspond AWS ER70S-6
YX 50-6 is Carbon steel MIG welding wire copper, using rich argon or carbon dioxide as shielding gas, wire melting fast,stable arc,small splash,strong anti-rush ability,small stomata sensitivity,excellent all-position welding,weld metal has good mechanical properties. Use for carbon steel and low alloy steel 500MPa grade single-channel and multi-pass welding. Such as the welding of containers, ships, vehicles, bridges, engineering machinery, steel structure and pressure vessels, also applies to the high speed welding of thin plate, pipeline steel.

Typical Chemical Composition (%)
Element C Mn Si S P Cr Mo Ni V Cu
Standard values 0.06~0.15 1.40~1.85 0.80~1.15 ≤0.035 ≤0.025 ≤0.15 ≤0.15 ≤0.15 ≤0.03 ≤0.5
Example values 0.07 1.58 0.86 0.011 0.016 0.016 0.03 0.017 0.006 0.15

Mechanical Properties of Deposited Metal:
Test Item Tensile Strength
RM/MPa Yield Strength
ReL/Mpa Elongation
A/% -30℃Impact Energy
KV2(J)
Standard values ≥500 ≥420 22 ≥27
Standard values 530 430 29 80
X-ray testing requirements: I Class

Note:
1、the protective gas by CO2 or Ar (80%) + O2 (20%) mixed gas, the gas flow rate 15 ~ 20L/min
2、 Welding ware stick-out length control in 10-18mm is appropriate。Control it in 20-25mm when current grater than 250A.
3、 The welding must completely remove rust, oil, water and other impurities.
l
4、 Sheet welding torch can be tilted to the side seam to reduce the penetration depth to avoid burn-through base metal.
5、 Outdoors construction wind speed 1.5m / s should take precautions to prevent blowholes defects.。
Quantity Per Month: 10000

Send your inquiry to this supplier

- Your message must be between 20-3000 characters.

Browse

- jpg, jpeg, gif, txt, doc, pdf, xls, docx,xlsx, rar or zip format;
- Max. size of 2MB